Pore in a Ti-2.5Fe blended elemental powder mixture sintered at 1200°C. Image taken with reflected light polarization contrast.
Pore in a Ti-2.5Fe blended elemental powder mixture sintered at 1200°C. Image taken with reflected light polarization contrast.